Advices for interior

Foaming or cracking

DESCRIPTION:
Blister formation resulting in small, round, concave depressions (cracks) when the blisters break into a paint film during application or paint drying.

 

CAUSES:

• Application of the product without leaving time to remove the air bubbles embedded as a result of more intense agitation
• Application of semi-glossy or glossy paints on a porous substrate

 

 SOLUTION:
The product will be brought to a temperature of 15-30 degrees C, before application.  Any film / bubbles formed at the surface of the product will be removed and the product will be homogenized. Grind the support with the appropriate grinding abrasive paper and dedust. The porous surfaces are first primed, followed by the application of the finishing coats.

NEWSLETTER
SUBMISSION
* In accordance with the GDPR, applicable from May 25, 2018, subscription involves
your explicit consent to the processing of your data for own purpose, for sending newsletters.
Contact Information
Constructorilor Boulevard, No. 1-3, Timisoara 300571, Romania
tel: 0040-256-222139
fax: 0040-256-222179